language

HUATAO GROUP
News & Events

We Help Customers To Meet The Great Challenges Of Our Time.

VIEW PRODUCTS
scroll down

Back to Overview

Dryer fabric for paper machines: spiral, woven and PPS

Nov 18,2026

Dryer fabric for paper machines: spiral, woven and PPS

A dryer fabric does a job nobody photographs. It runs inside the hot, damp, noisy dryer section, pressing the sheet against steam-heated cylinders so that the last water leaves the paper as vapour rather than staying in the fibre network. When it is right, the machine runs for weeks without anyone thinking about it. When it is wrong, you see it in the numbers within a shift: breaks at the first dryer group, a sheet that curls off the reel, steam demand that creeps up while production does not.

This guide is about choosing and looking after a dryer fabric for the kind of machines common in India, from Gujarat and Maharashtra packaging mills to the older waste-paper and agro-residue lines of Uttar Pradesh and Punjab: multi-cylinder, steam-heated, often built decades ago, running recycled-fibre or agro-residue furnishes into kraft, duplex and writing grades. It covers spiral versus woven construction, polyester versus PPS monofilament, how permeability should be read, what a dryer fabric suction roll expects from the fabric, and how cleaning and edge care decide whether a fabric lasts a full run or dies early.

Dryer fabric wrapping steam-heated cylinders

What a dryer fabric actually does

After the press section the sheet still carries a lot of water. Neither vacuum nor nip pressure removes it efficiently from that point on, so the web is taken around a series of steam-heated cast-iron or steel cylinders and the water is evaporated. The dryer fabric (also called dryer screen, dryer felt in older shop talk, or simply "the dryer") is the endless belt that wraps the cylinders together with the sheet. It has two jobs, and they pull in slightly different directions.

First, it holds the paper in firm contact with the hot cylinder surface. Contact is what transfers heat; a sheet that floats a millimetre off the shell dries slowly and unevenly. Second, it carries the sheet through the dryer section, which on an older machine with no vacuum assistance means the fabric is the only thing guiding the web through the open draws and around the lower cylinders. Both jobs have to be done while the fabric lets the evaporated moisture escape from the pocket. A fabric that is tight enough to press but too closed to breathe traps vapour against the sheet and slows drying; a fabric that breathes freely but presses weakly gives poor contact. Every choice in the rest of this guide is a way of balancing those two demands for a particular dryer group.

Dryer fabrics are used on packaging, cultural (writing and printing) and specialty machines alike. They are a different product from the felts upstream: a press felt works wet, with a batt structure designed around compaction, and that subject is covered separately in the press felt guide. A dryer fabric works hot, is made from monofilament or spun yarns in a woven or spiral structure, and its enemies are heat, steam, contamination and edge damage.

woven dryer fabric

The dryer section on Indian multi-cylinder machines: where each fabric runs

A cylinder dryer section is a line of steam-heated drums, usually 1.2 to 1.8 m in diameter on small and medium machines, arranged in groups. Each group is wrapped by one or two fabrics. Older Indian machines, many of them Fourdrinier or cylinder-mould lines, most often use a two-tier layout: an upper row and a lower row of cylinders, with the sheet zig-zagging between them. The upper fabric wraps the upper cylinders and carries the sheet over the felt-covered or bare guide rolls; the lower fabric does the same underneath. Between groups there are open draws, where the sheet travels unsupported for a short distance, and these are where most dryer-section breaks start.

Steam is not applied evenly. The first group is run cooler so the wet sheet is not shocked; the middle groups carry the highest steam pressure and do most of the evaporation; the last groups are brought back down to avoid overdrying and to let the moisture profile settle. A rule of thumb used on many machines is that cylinder steam pressure runs somewhere in the low single-digit bar range in the first group and noticeably higher in the middle groups, though the actual settings depend on grade, speed and condensate system. What matters for fabric selection is the consequence: the middle groups are the hot, humid, hydrolysis-prone positions, and the first and last groups are where the fabric's job is more about sheet handling than about surviving.

Dryer positionMain demand on the fabricTypical construction choice
First group (pre-dryer)Carry a weak, wet sheet; avoid marking; open enough to let steam from the wet sheet escapeOpen woven or spiral with good surface support
Middle groups (highest steam)Heat and hydrolysis resistance; stay clean and open under heavy evaporationPPS-reinforced woven or spiral where steam pressure is high
Final groupsDimensional stability; even contact so the sheet does not curl; gentle on dry paperPolyester, with permeability tuned to avoid over-drying
After-dryer / size press sectionSupport a re-wetted sheet that is weak again; resist starch or coating build-upEasy-to-clean woven or spiral; surface that sheds contamination

Spiral dryer fabric vs. woven dryer fabric

The two constructions are the central choice. A woven dryer fabric is made the way a textile is: warp yarns run in the machine direction, weft yarns cross them, and the structure is built up in one, two or more layers. It is woven flat, and then either joined with a pin seam (loops formed from the yarns at both ends, joined with a pintle wire on the machine) or woven endless. A spiral dryer fabric is something different: a series of continuous monofilament coils, each interlocked with its neighbour and held together by a straight pintle (or "link") yarn passed through the overlapping loops. It is not woven at all, and it has no machine direction warp in the usual sense.

Those construction differences produce real differences on the machine.

PropertyWoven dryer fabricSpiral dryer fabric
Open area and air flowControlled by yarn count and layer design; usually less open than a spiralVery open; vapour passes through the coils readily
Surface smoothnessCan be made quite smooth; good for light or delicate gradesCoarser; surface marking on lightweight sheets is more likely
Dimensional stabilityGood when properly heat-set; stretches little in serviceStable once installed, but depends on the pintle and coil joins
SeamPin seam or endless; the seam area needs careJoined across the width; no conventional seam mark
Cleaning behaviourFine structure can hold fines and stickies; needs regular showeringOpen coils shed contamination more easily and are simpler to clean
InstallationNeeds to be pulled through and seamed in positionBuilt from sections; can be laid in on a machine with little access

Where spiral construction earns its place

The open structure is the reason mills choose a spiral dryer fabric. Vapour leaves the pocket through the coils almost unimpeded, and contaminants fall out or wash out under a shower instead of locking into a dense weave. On machines that run waste paper or agro-residue furnishes, where sticky material and fine fibre pass through the press section and find the dryer fabric, that cleaning behaviour is practical rather than theoretical. Spirals are also the usual answer for the late dryer groups and for packaging grades where a rougher sheet surface is acceptable.

Installation is the other advantage that matters on old machines. A spiral fabric arrives as modules or lengths and is assembled on the machine, so it does not require threading a continuous belt through a tightly packed dryer frame with limited operator-side access. On machines where the frame is cramped, that is a genuine difference in downtime during a fabric change.

Where woven stays ahead

When sheet surface or light basis weight matters, a woven structure is safer. A finer, flatter face reduces marking, and a design with more machine-direction support can handle a weak sheet at the first group. Woven fabrics also tend to be the choice where very tight control of permeability is wanted, because yarn count and layer arrangement offer more adjustment than coil size does. The trade-off is that the finer structure is less forgiving of contamination: stickies and starch bridge the gaps sooner, and a woven fabric that is not showered regularly will lose permeability faster than a spiral running the same grade.

Neither construction is a universal upgrade over the other. The mill that gets it right usually looks at three things together: the grade (surface demands), the furnish (contamination), and the position on the machine (steam, humidity and sheet strength). A kraft liner machine and a writing-paper machine can reasonably end up with different answers on the same group.

Polyester vs. PPS dryer fabric: the hydrolysis question

The yarn material is the second main decision. Most dryer fabrics are made from polyester (PET) monofilament, which is strong, stable, tolerant of the temperatures in a normal dryer section and well understood. Its limit is hydrolysis. Polyester is a condensation polymer: given enough heat, moisture and time, water molecules attack the chemical bond in the polymer chain, the filament loses molecular weight, and it becomes brittle. A hydrolysed polyester yarn can look almost normal and then snap when the fabric is flexed over a guide roll or when you try to take it off.

PPS (polyphenylene sulphide) is a different polymer. It does not hydrolyse under dryer-section conditions, so it keeps its strength where polyester degrades. It is also less flexible, harder to weave and heavier to handle, which is why it is used where it is needed and not as a default. In Huatao's description of its range, polyester fabrics are intended for normal paper machine conditions, and PPS-reinforced fabrics for hydrolysis-prone positions where high steam pressure is used.

FactorPolyester (PET)PPS
Behaviour in hot, humid pocketsSlowly hydrolyses; strength loss accelerates with temperature and moistureDoes not hydrolyse under these conditions
Typical useMost dryer positions on standard machinesHot middle groups with high steam pressure; closed or poorly ventilated pockets
Flexibility and weavabilityExcellentStiffer; used selectively, often as a reinforcement within a polyester design
Failure mode when pushedBrittle yarns, edge cracking, seam failureRarely brittle; wear or contamination usually decides life

Which machines are really exposed?

Hydrolysis is a combination problem. Heat alone does not do it, and neither does moisture alone. A fabric in a hot, humid pocket that is closed off by a hood or by neighbouring cylinders is the typical victim. On older Indian machines the usual contributing factors are poor condensate removal (so cylinder surfaces run hotter than the steam-pressure gauge suggests), pockets with limited ventilation, and operation at the upper end of the machine's speed range for a long time. A pH that drifts well away from neutral in the sheet or in the contaminants carried on the fabric can accelerate the damage as well. If a polyester fabric on the third group keeps failing with brittle yarns at around the same running time every change, that is hydrolysis, not wear, and the remedy is a change of material or a change of ventilation, not a tighter cleaning schedule.

Check this first: before specifying PPS on a position, confirm the steam pressure and condensate removal on that group. A cylinder with a flooded shell can dry badly and run hotter at the surface, and a fabric upgrade will not repair either problem. PPS is a remedy for a hot, humid position, not for a drying problem caused elsewhere.

Dryer fabric permeability: what the number means

Air permeability is the figure most buyers ask about first, usually stated in cubic feet per minute per square foot (CFM) or in cubic metres per square metre per hour. It is measured by pulling air through a sample at a fixed pressure drop and reading the flow. It is a useful comparison number, but it is a laboratory number, and what matters on the machine is how the fabric ventilates the pocket and what the permeability becomes after it has been running for a while.

As a broad order of magnitude, open spiral fabrics sit at the high end of the range and dense woven structures at the lower end, with a wide spread within each. The table below is the way mills commonly frame it.

Typical industry reference values

Open spiral dryer fabricHigh air flow; open coil structure
Woven, open designMedium to high air flow
Woven, dense designLower air flow; smoother sheet side
Permeability measured onNew, clean sample at standard pressure drop
Permeability in serviceFalls as fines, stickies and starch fill the structure
Machine position, hot middle groupsHigher permeability favoured to clear vapour
Machine position, first and last groupsModerate permeability favoured for sheet support

Dryer fabric and the suction roll

Many dryer sections, including a number of rebuilt machines in India, have one or more vacuum or suction rolls in the dryer section, typically at the first cylinders or at the lower rolls where the sheet reverses direction. The suction roll pulls air through the fabric and the sheet to hold the web against the fabric through the open draw, which cuts down on flutter and breaks. Where a dryer fabric suction roll is fitted, the fabric and the roll are a pair, and they have to be matched.

The fabric must be permeable enough that the vacuum actually reaches the sheet. A dense fabric on a suction roll acts like a lid: the pump runs, the gauge reads vacuum, and very little holding force arrives at the sheet. A fabric that is too open does the opposite: air passes freely, the vacuum level falls, and the sheet is held weakly. When a mill asks why a new fabric has caused more breaks at the suction roll position, the permeability mismatch is the first thing to check, ahead of anything about the roll itself.

Cleaning and contamination on Indian furnishes

The furnish decides how quickly a dryer fabric fouls. Recycled fibre from mixed waste carries residual adhesives, wax, coating fragments and starch. Agro-residue pulps, such as bagasse and wheat straw, bring fine particles, silica-rich fines and residual liquor. Machines that run a mix, as many do through the year as raw-material availability shifts with the season, see contamination that varies from week to week. The fabric picks up whatever the sheet carries with it into the dryer, and the heat bakes it on.

Online cleaning

A high-pressure cleaning beam or an oscillating spray shower directed at the fabric's return run is the standard way to keep the structure open. Water at the right pressure displaces fines and stickies; used correctly, it keeps permeability close to its starting value and removes the need for chemical cleaning. Showers have to be set up with care: a nozzle that sits too close or runs at too high a pressure can damage the yarns or loosen the edge reinforcement. A beam that does not traverse leaves stripes. A fabric that does not dry enough before it re-enters the pocket may carry water into the next cylinder and bring on a different problem.

Shop-floor tip: log permeability readings at fixed positions on every fabric. A table of three or four readings per week is enough. The trend tells you whether the cleaning regime is adequate far sooner than visual inspection does, because a fabric can look clean and still have lost a third of its air flow.

Edge reinforcement, tension and guiding

Most dryer fabrics do not die in the middle. They die at the edges, or at the seam. An edge is exposed to the hot, dry atmosphere beyond the sheet, to the cylinder end shoulders and to guide-roll flanges, and it is where the fabric has to cope with lateral movement. Edge reinforcement is therefore a design feature, not a refinement: a stronger or sealed edge resists fraying, cracking and yarn pull-out, particularly where the fabric rubs against fixed objects. Where edges fray, loose filaments lift into the pocket, wrap on the cylinder or guide roll and can score the shell.

Guiding

Dryer fabrics wander. Variation in tension across the width, a guide roll that is slightly out of parallel or a build-up on a roll surface moves the fabric sideways. An automatic fabric guide corrector holds the fabric on track by steering a guide roll in response to a sensor on the fabric edge; pneumatic types are common on paper machines and are used on forming fabrics, press felts and dryer fabrics alike. If a fabric is regularly running to one side and the guide corrector is working hard to compensate, the right answer is to fix the root cause, whether that is roll alignment, uneven cylinder expansion or a tapered build-up on a roll, rather than letting the guide take the load indefinitely. A guide that is permanently at the end of its travel can no longer protect the fabric at all.

Dryer fabrics on Indian paper machines: monsoon, old dryer sections and agro furnishes

An Indian dryer section works under conditions that textbooks written for temperate, mainly virgin-fibre mills rarely describe. Many mills in Gujarat, Maharashtra, Tamil Nadu, Uttar Pradesh and Punjab run Fourdrinier or cylinder-mould machines at low to medium speed on kraft, testliner, fluting, duplex board and writing and printing grades. Those machines often carry a dryer section extended over the years, with cylinders of mixed age, uneven condensate removal and pockets that were never designed with ventilation in mind.

Monsoon humidity and summer heat

In the monsoon months the air drawn into the machine hall is already close to saturation, so the pocket has less capacity to take up evaporated water. A fabric that was adequately open in January starts to hold vapour in July, and operators see it as slower drying and more steam. In the hot months the opposite problem appears: hall temperature rises, fabric and yarn run hotter, and a polyester fabric on a hot middle group reaches its hydrolysis limit earlier. For an Indian machine the fabric choice for the hottest groups should therefore be made with both seasons in mind, and permeability checks are worth doing more often when the weather changes.

Waste paper, bagasse and wheat straw

Indian waste-paper mills (OCC and mixed grades) send stickies, wax and starch into the dryers, while bagasse and wheat-straw lines send fine particles that settle in the structure and bake in. These are the reasons an open spiral dryer fabric is so often chosen on Indian packaging machines, and why a woven fabric on the same machine needs a disciplined shower routine. Sticky patches that appear a few days after a change of waste-paper source are a stock-preparation signal as much as a fabric one.

Steam supply and condensate

Boilers fired on coal, biomass or husk give steam pressure that wanders through a shift. Cylinders that lose pressure then recover it cause sudden temperature swings at the fabric. Combined with weak siphons or flooded cylinders, this produces the early hydrolysis failures many Indian mills blame on the fabric. Fix the condensate system first; then decide whether the position needs PPS.

For Indian mills: keep a simple seasonal log. Record fabric permeability, steam pressure by group and the furnish blend at the start of the monsoon, mid-season and the hot months. After one year the pattern of when your fabrics blind or hydrolyse will be clearer than any general guideline.

Common dryer fabric problems and what they point to

Dryer fabric faults often look similar from the operator's platform. The table pairs the visible symptom with the cause most worth checking first.

SymptomLikely causeFirst check
Steam demand rising with no change in productionPermeability loss; pocket no longer ventilatingMeasure air permeability at several widths; review shower function
Breaks at the first open drawFabric too open or too closed at that position; poor sheet supportCompare permeability with the earlier fabric; check suction roll vacuum
Brittle yarns, edge cracking after a few monthsHydrolysis on a hot, humid positionCheck steam pressure and condensate removal; consider PPS reinforcement
Fabric tracking to one sideRoll misalignment or uneven tensionCheck parallelism and guide corrector travel
Sticky patches or dark spots on the fabricStickies or contamination from the furnishReview stock-preparation screening; check shower pressure and position
Fraying at the edgeEdge rubbing on guide flanges; inadequate edge protectionCheck guide-roll flanges and edge clearance
Paper curl or uneven moisture profile across the reelUneven drying; edges more contaminated than the centreTest edge versus centre permeability; clean edges
Surface marks on the sheetCoarse structure or seam mark on a light gradeReview weave choice; inspect the seam

Curl deserves a closer look because it is often blamed on the paper rather than the fabric. When one side of the sheet dries faster than the other, the sheet curls toward the drier side. A fabric that dries unevenly across the width because of partial blinding produces uneven moisture and cross-direction curl. The remedy is not to add more steam but to restore even permeability.

How to specify and replace a dryer fabric

When you ask a supplier for a dryer fabric, a few facts shorten the conversation considerably. They are the same facts an engineer would ask for when assessing a problem.

Give the supplier the machine and position, cylinder diameter and wrap path (confirmed against the fabric being removed), grade and speed, furnish, steam pressure by group, and above all the failure history of the last fabric, with photographs of the damage.

Deciding when to replace

Dryer fabric life is never a fixed number of days. It depends on the position, the material, the furnish, the cleaning regime and how well the edges and seam are cared for. Plan changes around evidence rather than the calendar: permeability that can no longer be recovered by cleaning, an edge or seam that has begun to fail, loss of dimensional stability so the fabric no longer tracks, or a rise in breaks that points back to the fabric. Changing a fabric a few days before it fails, at a planned stop, is almost always better than changing it after a break during a run.

Dryer fabrics are not the only clothing on the machine: the wet end runs on forming fabric, and downstream of the dryers the sheet goes to calender machines, then the pope reel, where an uneven moisture profile from the dryers shows up as soft edges or curl.

Huatao Group dryer fabric for Indian paper machines

Huatao Group offers dryer fabrics in two series, spiral and woven, and describes the range as covering all the dryer fabrics needed on paper and board machines. Its stated uses are packaging paper machines, cultural paper machines and specialty paper machines, which maps directly onto the kraft, testliner, writing and printing lines described above. The points below follow the product information and are given here with what each means on an Indian machine.

  • Spiral and woven series. A mill can match the construction to the position: spiral on the later groups of a waste-paper or agro-residue packaging machine where contamination is the main enemy, woven where a lighter sheet needs a smoother face.
  • Polyester for normal conditions, PPS-reinforced for hydrolysis-prone positions with high steam pressure. On Indian machines this separates the ordinary groups from the hot middle groups, especially those fed by uneven boiler steam in summer.
  • Resistance to hydrolysis, wear and jam resistance for long life. Relevant where humid pockets and abrasive agro fines both attack the fabric.
  • High contact surface area and good heat transfer, with increased ventilation. The product information links this to lower energy use, which matters on cylinder sections starved of steam in peak production.
  • Fewer paper breaks and fewer temporary shutdowns. The practical gain on low-speed machines whose breaks cluster at open draws.
  • Good dimensional stability, ease of cleaning and flexible, strong edge reinforcement. Useful on machines with worn guiding, and on furnishes that foul the fabric edge.
  • Perfect seam and seaming aids for easy installation. Helpful where access to a cramped, older dryer frame is limited during a change.

The product information gives no numerical range for dryer fabrics, so the reference values earlier in this guide are general industry guidance, not product claims. For a specific Indian machine, the position, steam pressure and furnish decide the series and material, and Huatao can be consulted with those details.

Frequently asked questions

Is a spiral dryer fabric better than a woven one for a waste-paper kraft machine?
Often it is the practical choice, but it is not automatic. Recycled furnishes carry stickies, starch and fine particles that block a dense woven structure quickly, and the open coils of a spiral fabric shed that material more readily and clean up better under a shower. Against that, a spiral surface is coarser, and a very light sheet at the first group may need a woven face for support. Most kraft and testliner machines in India, including many waste-paper mills in Gujarat and Punjab, do well with spiral fabrics on the later groups and a woven or finer-structure fabric where the sheet is still weak.
How can I tell whether a dryer fabric failed from hydrolysis or from ordinary wear?
Look at the yarns. Hydrolysed polyester is brittle: the monofilaments snap cleanly when bent, edges crack rather than fray, and the fabric may feel stiff and dry even while still looking whole. Ordinary wear shows as thinning, flattened knuckles and polished surfaces on the running side. Hydrolysis also tends to occur at the same running time on the same position each change, usually on a hot middle group. If the pattern repeats, check steam pressure and pocket ventilation, and consider a PPS-reinforced fabric for that position.
What does dryer fabric permeability tell me, and how often should I measure it?
Permeability shows how freely air, and therefore vapour, can pass through the fabric. A new fabric reads high; a fouled one reads lower. Measuring it at several positions across the width at each planned stop, and logging the values, shows the trend long before the fabric looks dirty. A steady decline means the cleaning regime is not keeping up. A difference between edge and centre points to edge build-up. The number is a comparison tool, so use it against the fabric's own starting value rather than against another mill's reading.
Why do breaks increase after a new dryer fabric is fitted next to a suction roll?
The usual cause is a permeability mismatch. A suction roll holds the sheet by pulling air through the fabric. If the new fabric is denser than the old one, very little vacuum reaches the sheet, and the web flutters in the open draw. If it is far more open, vacuum drops and holding force falls. Compare the new fabric's air permeability with that of the previous fabric, check vacuum at the roll, and inspect the shell holes and box seals for wear or leakage before blaming the fabric design.
Does a cylinder dryer section need a different fabric for every group?
Not necessarily. Many machines run one polyester grade on most groups and reserve a PPS-reinforced or more open fabric for the one or two hot middle groups where life has been short. The first group usually wants good sheet support, and the last groups want even contact so the sheet does not curl. A useful approach is to start from the failure history: change only the positions that have failed or cause breaks, rather than redesigning the entire dryer section at once.
Does monsoon humidity change which dryer fabric an Indian mill should choose?
It changes how you run it more than which one you buy. During the monsoon the hall air holds little extra moisture, so a fabric that was only just open enough in winter starts to hold vapour and steam demand rises. In the hot months the pockets run hotter and polyester on the highest-steam groups ages faster. Indian mills do best to measure permeability more often when the season turns, keep showers working at the edges, and reserve PPS-reinforced fabric for the groups that have actually shown hydrolysis. Ventilation and hood air balance on the machine matter as much as the fabric itself.
Why do dryer fabrics on bagasse and wheat-straw machines in India blind so quickly?
Agro-residue pulps carry fine particles and silica-rich fines that are not fully removed in washing and screening. They pass through the press section, settle into the dryer fabric and are baked in by the heat, closing the openings and cutting permeability. An open spiral fabric sheds more of this material and responds better to showering, while a dense woven face fills sooner. Keep the shower aimed at the return run, check edges separately, and look at the washing and screening stages upstream when blinding gets worse after a change of raw material. Uneven blinding also gives uneven drying and curl across the sheet.